incoloy800 is an alloy that typically contains 15-25% Cr, 30-45% nickel, and small amounts of aluminum and titanium.
800 alloy from high temperature and rapid cooling are in the austenite single zone, therefore, the use of a single austenite structure. The alloy has a high chromium content and sufficient nickel content, so it has a high temperature corrosion resistance, and is widely used in industry.
Product description:
INCOLOY 880/880H/880HT is a high-strength, corrosion-resistant nickel-iron-chromium alloy designed for high-temperature applications. It offers exceptional resistance to oxidation, carburization, and sulfidation, making it ideal for harsh industrial environments. With its high nickel and chromium content, it exhibits excellent resistance to corrosive media, including acids and chloride solutions. The alloy’s unique microstructure provides outstanding mechanical properties, ensuring reliable performance under extreme conditions. Widely used in chemical processing, petrochemical, and power generation industries, INCOLOY 880/880H/880HT is a reliable choice for high-temperature applications that demand both strength and corrosion resistance.
Product characteristics:
800 alloy has the following properties
1. Good corrosion resistance and high temperature resistance
2. Good mechanical properties at minus zero, room temperature and up to 600°C
3. Good anti-oxidation, reduction, nitriding environmental performance
4. Good processing performance
The 800H alloy has the following characteristics
1. Excellent corrosion resistance in water-based media at extremely high temperatures of up to 500℃
2. Good resistance to stress corrosion
3. Good processability
Chemical composition:
Alloy | % | C | Mn | Si | Cr | S | Ni | Cu | Fe | Al | Ti |
800 | Min | – | – | – | 19 | – | 30 | – | Bal. | 0.15 | 0.15 |
Max | 0.10 | 1.5 | 1 | 23 | 0.015 | 35 | 0.75 | Bal. | 0.60 | 0.60 | |
800H | Min | 0.05 | – | – | 19 | – | 30 | – | Bal. | 0.15 | 0.15 |
Max | 0.10 | 1.5 | 1 | 23 | 0.015 | 35 | 0.75 | Bal. | 0.60 | 0.60 | |
800HT | Min | 0.06 | – | – | 19 | – | 30 | – | Bal. | 0.15 | 0.15 |
Max | 0.10 | 1.5 | 1 | 23 | 0.015 | 35 | 0.75 | Bal. | 0.60 | 0.60 | |
Al+Ti为0.85-1.20 |
Physical property:
density | 8.0G/CM³ |
Fusing point | 1350-1400C |
The minimum mechanical properties of an alloy at room temperature:
Alloy state | Tensile strength | Yield strength | Rate of elongation | ||||
RM N/MM2 | RP0.2N/MM2 | A5 % | |||||
800 | 500 | 210 | ≤35 | ||||
800H | 450 | 180 | ≤35 |
Product form and implementation standards:
Product | ASTM standards | ASME standards | AME standards | ||||
Sheet. Sheet. Strip | B409 | SB409 | 5871 | ||||
Seamless pipe | B163.B407 | SB163.SB407 | |||||
Welded pipe | B514 | ||||||
Bar. Cake | B408 | SB408 | |||||
forging | B564 | SB564 |